This table outlines the core specifications of 45# Angle Steel 120x120mm, a medium-carbon steel profile valued for its balanced strength, machinability, and cost-effectiveness. Its 120x120mm equal-leg design makes it ideal for heavy-duty structural roles requiring reliable load distribution.

whatsapp

wechat

2010 ESTABLISHED

410 EMPLOYEE

363+CLIENTS

13000+ trade

Why Choose Baosteel®

Never stop the technological innovation,more than 50 patents, so that every piece of Products becomes the masterpiece.From consulting to after-sales support, theall-weather, all-process, all-round, whole-hearted service system will Escort for you.

 

Product details

45# Angle Steel 120x120mm is a robust medium-carbon structural steel profile, engineered to deliver a balanced combination of strength, machinability, and affordability for industrial, construction, and machinery applications. With its substantial 120x120mm equal-leg design and optimized carbon content, this angle steel provides reliable load-bearing performance, making it a go-to choice for medium to heavy-duty structural frameworks and mechanical components.
Parameter Value/Description Unit Remarks
Material 45# (Medium-Carbon Structural Steel) Chemical Composition: C 0.42–0.50%, Si 0.17–0.37%, Mn 0.50–0.80%, P ≤0.035%, S ≤0.035%
Section Size 120×120 mm Equal-leg angle, both legs 120mm
Thickness Options 10/12/14/16/18 mm Standard available thicknesses
Weight per Meter 18.2/21.6/25.0/28.3/31.5 kg/m Corresponding to 10/12/14/16/18mm thickness
Length 6000–12000 (Customizable) mm Standard 6m/9m; cut-to-order available
Cross-Sectional Area 23.117 (10mm) cm² Example value; varies with thickness
Tensile Strength (As-rolled) 600–750 MPa Typical range at room temperature
Tensile Strength (Heat-treated) ≥630 MPa Minimum after quenching and tempering
Yield Strength (Heat-treated) ≥355 MPa Minimum after quenching and tempering
Elongation (δ5) ≥16 % Minimum at room temperature (as-rolled)
Hardness (As-rolled) 197–241 HBW Brinell hardness range
Hardness (Heat-treated) 22–28 HRC Achievable range via quenching + tempering
Impact Toughness (αk) ≥39 J/cm² Minimum at room temperature (heat-treated)
Heat Treatment Quenching (840°C, water cooling) + Tempering (600°C, air cooling) Optional process to enhance strength/toughness
Manufacturing Standard GB/T 699-2015 Compliant with Chinese standard for high-quality carbon structural steels
Surface Treatment Mill finish (black) / Paint coating / Zinc plating Custom finishes available for corrosion protection
Typical Applications Machinery frames, structural bracing, gear blanks, connecting rods, heavy-duty brackets Suitable for medium-load structural and mechanical components